IIUM Repository

Fracture fixation plates for fracture healing: comparing 316L stainless steel by metal injection molding technique plate with conventional plate in rabbit fracture model

Mohd Jan, Nurul Hafiza and Zulkifly, Ahmad Hafiz and Ibrahim, Mohd Zulfadzli and Omar, Mohd Afian and Abdul Jalil, Rosnani and Shaharudin, Aliah and Mat Nor, Rabiatul Adawiyah and Syed Mohamed, Syarifah Saffa 'Aina and Che Seman, Che Nor Zarida and Abdul Jalil, Normila (2012) Fracture fixation plates for fracture healing: comparing 316L stainless steel by metal injection molding technique plate with conventional plate in rabbit fracture model. Regenerative Research, 1 (Supplement Issue). p. 62. E-ISSN 2232-0822

[img] PDF - Published Version
Restricted to Registered users only

Download (594kB) | Request a copy

Abstract

Metal injection molding (MIM) combines the material flexibility of powder metallurgy and the design flexibility of plastic molding. With properties comparable, or better than, those of wrought steel, the MIM process are ideally suited to producing small and complex-shaped parts with outstanding mechanical properties. In addition to that, implants produced via this process have high final density and close porosity. This is an innovation to produce new orthopaedic fracture implants and it also can be used to device new special orthopaedic implants. The cost for the technique is cheaper when compared to the conventional technique. The objective is to evaluate the plate function in fracture using New Zealand White (NZW) rabbits. Evaluation was done at three, six, nine, twelve and twenty six weeks by using radiograph evaluation. The procedure commenced with pre-operation, intra-operative and post-operation sessions. There were three groups of experimental studies; Group O Sham group as control, Group 1; (fracture midshaft tibial implant with conventional plate by Synthes), Group 2; (fracture midshaft tibial implant with MIM plate). Both showed similar results as a method to hold the fracture fragments. X-Rays showed that callus formation occured in both groups (Conventional and MIM groups) of fracture site at three, six, nine and twelve weeks. Bridging was noted at six weeks. There is no infection noted in both groups with no adverse effects. Fracture union noted in all groups. These results revealed that MIM showed comparable function capabilities as the conventional plate to hold the fracture fragments and promote immobilization for fracture healing process.

Item Type: Article (Journal)
Additional Information: 2397/57863
Uncontrolled Keywords: Metal Injection Molding,fracture fixation plate, 316L stainless steel
Subjects: R Medicine > RD Surgery > RD701 Orthopedics
Kulliyyahs/Centres/Divisions/Institutes (Can select more than one option. Press CONTROL button): Kulliyyah of Medicine > Department of Department of Orthopaedics, Traumatology & Rehabilitation
Depositing User: Mr. Mohd Zulfadzli Ibrahim
Date Deposited: 04 Aug 2017 16:51
Last Modified: 04 Aug 2017 16:51
URI: http://irep.iium.edu.my/id/eprint/57863

Actions (login required)

View Item View Item

Downloads

Downloads per month over past year